Scaffolds were fabricated by electrospinning using polycaprolactone (PCL) blended with poly(methyl methacrylate) (PMMA) in ratios of 10/0, 7/3, 5/5 and 3/7. The PCL/PMMA ratio affected the fiber diameter, contact angle, tensile strength and biological in vitro and in vivo properties of the scaffolds, and the 7/3 ratio resulted in a higher mechanical strength than 5/5 and 3/7. In vitro cytotoxicity and proliferation of MG-63 osteoblast cells on these blended scaffolds were examined by MTT assay, and it was found that PCL/PMMA blends are suitable for osteoblast cell proliferation. Confocal images and expression of proliferating cell nuclear antigen confirmed the good proliferation and expression of cells on the 7/3 PCL/PMMA fibrous scaffolds. In vivo bone formation was examined using rat models, and bone formation was observed on the 7/3 PCL/PMMA scaffold within 2 months. In vitro and in vivo results suggest that 7/3 PCL/PMMA scaffolds can be used for bone tissue regeneration.

키워드

PMMA; PCL; electrospinning; bone regeneration; DRUG-DELIVERY; PCL SCAFFOLDS; PMMA; METHACRYLATE; FABRICATION; COMPOSITES; NANOFIBERS; PLGA
제목
In vitro and in vivo evaluation of electrospun PCL/PMMA fibrous scaffolds for bone regeneration
저자
Son, So-Ra; Nguyen-Thuy Ba Linh; Yang, Hun-Mo; Lee, Byong-Taek
DOI
10.1088/1468-6996/14/1/015009
발행일
2013-02
유형
Article
저널명
Science and Technology of Advanced Materials
권
14
호
1